2205 |
|
Tensile strength (min) |
655 MPa |
0.2% Proof Strength (min) |
450 MPa |
Elong. (in 50mm) (min) |
25% |
Hardness (max) |
293 HB |
Grade | UNS No | C % | Cr % | Ni % | P % | Si % | S % | Mo % | N % | Mn % |
2205 | S32205 | 0.03 | 22.0-23.0 | 4.5-6.5 | 0.03 max | 1 max | 0.02 max | 3.0-3.5 | 0.14-0.20 | 2.0 |
Density (Kg / M3) | Modulus of Elasticity (GPa) | Poisson’s Ratio | Thermal Conductivity (W/moC) | Thermal Capacity (I/KgoC) | Electrical Resistivity |
7800 | 200 | 0.3 | 15 | 500 | 0.80 |